TECARAN ABS
Ensinger TECARAN™ ABS is a terpolymer and an amorphous resin. It is manufactured by combining three different compounds. The three that make up TECARAN™ ABS are acrylonitrile, butadiene, and styrene. TECARAN™ ABS occupies the unique position of being a bridge between the commodity and other higher performance engineering thermoplastics. Its performance is characterized by toughness and impact strength even at low temperatures, good stiffness and machinability.
- Cost Effective
- Good Toughness At Low Temperatures
- Easily Machinable
- Natural Is Made From Resin That Is FDA, USDA, 3A Dairy Compliant
- Available In Natural or Black
- Meets ASTM D4673-02 ABS220B44500
- Easily Bonded
The applications for TECARAN™ ABS range from Aerospace and automotive parts and housings, to parts for agricultural lawn and garden equipment and components for medical and business equipment, as well as many others.
| Properties | ASTM Test Method | Units | TECARAN™ ABS |
|
|---|---|---|---|---|
| Physical |
Density
|
D792 | lbs/in3 | 0.0380 |
|
Specific Gravity (gm/cm3)
|
D792 | g/cc | 1.04 | |
|
Water Absorption, @24 hours, 73°F
|
D570 | % | 0.30 | |
|
@Saturation, 73°F
|
D570 | % | 0.70 | |
| Mechanical |
Tensile Strength @ Yield, 73°F
|
D638 | psi | 5,100 |
|
Tensile Modulus
|
D639 | psi | 270,000 | |
|
Elongation @ Break, 73°F
|
D638 | % | 15 | |
|
Flexural Strength, 73°F
|
D790 | psi | 8,000 | |
|
Flexural Modulus, 73°F
|
D790 | psi | 270,000 | |
|
Compressive Strength,
|
D695 | psi | - | |
|
Izod Impact, Strength, 73°F
|
D256 | ft-lbs/in | 6.3 | |
|
Rockwell Hardness, 73°F
|
D785 | R Scale | 102 | |
|
Shure Hardness
|
D Scale | - | ||
|
Wear Factor Against Steel, 40 psi, 50 fpm
|
D37012 | in3 1 --- x --- hr PV |
3,500 x 10-10 | |
|
Static Coefficient of Friction
|
D3702 | 0.19-0.21 | ||
|
Dynamic Coefficient of Friction, 40 psi, 50 fpm
|
D3702 | 0.35 | ||
| Thermal |
Heat Deflection Temperature @ 66 psi
|
D648 | °F | 210 |
|
@ 264 psi
|
D648 | °F | 198 | |
|
Coefficient of Linear Thermal Expansion
|
D696 | in/in/°F | 5.2 x 10-5 | |
|
Maximum Servicing Temperature, Intermittent
|
- | °F | 210 | |
|
Long Term
|
UL746B | °F | 160 | |
|
Specific Heat
|
C177 | BTU/lb-°F | 0.28 | |
|
Thermal Conductivity
|
UL94 | - | 1.18 | |
|
Vicate Softening Point
|
- | °F | 220 | |
|
Melting Point
|
D2133 | °F | - | |
|
Flammability
|
UL94 | - | HB | |
| Electrical |
Surface Resistivity
|
D257 | ohm/square | - |
|
Volume Resistivity
|
D257 | ohm-cm | 10 x 1015 | |
|
Dielectric Strength
|
D149 | V/mil | 450 | |
|
Dielectric Constant, @ 60 Hz, 73°F, 50% RH
|
D150 | 3.3 | ||
|
@ 1 MHz
|
D150 | - | ||
|
@ 20 GHz
|
D150 | - | ||
|
@ 30 GHz
|
D150 | - | ||
|
Dissipation Factor @ 60 Hz, 73°F
|
D150 | 0.02 | ||
| This information is only to assist and advise you on current technical knowledge and is given without obligation or liability. All trade and patent rights should be observed. All rights reserved. Values obtained from extruded samples. TECARAN™ - Ensinger Industries, Inc. |
||||