TECANYL MT (medical grade)
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease and tool friendliness of acetal or POM. This allows part designers to take advantage of lower manufacturing costs by increasing output rates, and reducing tool wear, all without sacrificing part performance. TECANYL™ MT and TECANYL™ MT XRO™ shapes are all ISO 10993 tested to support their use in instrumentation that is intended to come in contact with blood and tissue for a period of not more than 24 hours. Ensinger can also provide TECANYL™ MT grades in finished injection molded parts for high volume applications.
- Excellent autoclave performance comparable to higher temperature materials
- Easily machined, producing high quality surface
- No black speck generation as in sulfone polymers
- Lower manufacturing costs
- ISO 10993 Tested
TECANYL™ MT exhibits a broad range of outstanding properties for applications in medical devices where exposure to extreme heat and hygienic measures are demanded. Excellent wear properties, ease of quality machining and availability in a wide range of colors contribute to its desirability in medical devices.
| Properties | ASTM Test Method | Units | TECANYL™ MT |
TECANYL™ MT XRO |
TECANYL™ MT CF30 |
|
|---|---|---|---|---|---|---|
| Physical |
Density
|
ISO 1183 | lbs/in3 | 0.03 | 0.03 | - |
|
Specific Gravity
|
D792 | - | 1.08 | 1.08 | 1.12 | |
|
Water Absorption, equilibrium, 73°F
|
ISO 62 | % | 0.23 | 0.23 | - | |
|
@saturation, 73°F
|
- | - | - | - | - | |
| Mechanical |
Tensile Strength @ Break, 73°F
|
D638 | psi | 9,800 | 9,800 | 20,600 |
|
Tensile Modulus, 73°F
|
D638 | psi | 471,000 | 471,000 | - | |
|
Elongation @ Break, 73°F
|
D638 | % | 16.3 | 16.3 | 5.94 | |
|
Flexural Strength, 73°F
|
D790 | psi | 14,600 | 14,600 | 38600 | |
|
Flexural Modulus, 73°F
|
D790 | psi | 368,000 | 368,000 | 3,027,200 | |
|
Compressive Strength
|
- | - | - | - | - | |
|
Izod Impact Strength, Notched, 73°F
|
D256 | ft-lbs/in | 2.6 | 2.6 | 1.14 | |
|
Rockwell Hardness, 73°F
|
- | - | - | - | - | |
|
Shore Hardness
|
- | - | - | - | - | |
|
Wear Factor Against Steel, 40 psi, 50 fpm
|
- | - | - | - | - | |
|
Static Coefficient of Friction
|
- | - | - | - | - | |
|
Dynamic Coefficient of Friction, 40 psi, 50 fpm
|
- | - | - | - | - | |
| Thermal |
Heat Deflection Temperature @ 66 psi
|
- | - | - | - | - |
|
@264 psi
|
D648 | °F | 296 | 296 | 296 | |
|
Coefficient of Linear Thermal Expansion (-40°F to
|
E831 | in/in/°F | 4.81-10-5 | 4.81-10-5 | 4.81-10-5 | |
|
100°F)
|
- | °F | - | - | - | |
|
Maximum Servicing Temperature, Intermittent
|
- | °F | - | - | - | |
|
Long Term
|
- | - | - | - | - | |
|
Specific Heat
|
- | - | - | - | - | |
|
Thermal Conductivity
|
ISO 306 | °F | 168 | 168 | 168 | |
|
Vicat Softening Point, Rate B/50
|
- | - | - | - | - | |
|
Applicable Temperature Range for Thermal Expansion
|
- | - | - | - | - | |
| Electrical |
Surface Resistivity
|
- | - | - | - | - |
|
Volume Resistivity
|
- | - | - | - | - | |
|
Dielectric Strength
|
- | - | - | - | - | |
|
Dielectric Constant, @ 60 Hz, 73°F, 50% RH
|
- | - | - | - | - | |
|
Dissipation Factor, @ 60 HZ, 73°F
|
- | - | - | - | - | |
|
|
- | - | - | - | - | |
|
|
- | - | - | - | - | |
|
|
- | - | - | - | - | |
| This information is only to assist and advise you on current technical knowledge and is given without obligation or liability. All trade and patent rights should be observed. All rights reserved. NORYL® - Sabic. TECANYL™MT - Ensinger Industries, Inc. XRO™ - Ensinger Industries, Inc. |
||||||